I’ve been noticing some delamination (layer separation), but only on solid infill and top layers, and only on larger surfaces
Initially, I tried reducing speed, but didn’t notice any improvement
There are no noticeable issues on short lines, so I think this is something to do with acceleration, which I didn’t realise was a thing, but there are indeed settings for this in OrcaSlicer
Update:
Reducing acceleration does seem to have resulted in less severe delamination, but it hasn’t gone away completely
So I think I need to reduce it just a little bit more
jokeyrhyme@lemmy.mlOPEnglish2·7 days ago- Sovol3D SV06 ACE
- OrcaSlicer recently gained a built-in profile for exactly this model, and I’ve had all sorts of issues since switching to that profile (previously I started with a generic printer profile)
- the new profile is fine on PLA, but PETG is what I’m currently using
- yeah, I only just learnt about the print visualisation feature, the delamination does seem to frequent the same place on the object/plate
- it’s the 6x6 panel from https://www.printables.com/model/859807-print6-panels
- the spans from cross hole to cross hole are short and never delaminate
- the long straight edge-to-edge spans that dodge the holes have been troublesome
- the plan is to reduce acceleration a bit more, and then (if that doesn’t help) reduce speed a bit (I’ve already reduced speed and filament volume anyway because of PETG)